In fact, the sheet should be one of the most important parts. The quality of a piece of plate can be defined from four attributes: quiet zone strength, water swelling rate, formaldehyde emission, and screw holding force. Why are these four attributes important? Let's explain it in detail for everyone:
Static bending strength
What is the intensity of static bending? In a word, the intensity of static bending is an important attribute that determines whether your cabinet will bend or even break during later use.
The static bending strength of the board is related to the raw material. Generally speaking, the physical properties of the wood grown in the alpine forest area are more stable. If the age of the tree is too short, the value of the static bending intensity will be low, so the age of the tree is about 15-30 years. In addition, the production process can also have an important impact on the static bending strength of the sheet. A reasonable process can make the sheet structure stable and not easy to warp and deform.
Of course, in fact, the deformation of the cabinet of the cabinet is related to the strength of the static bending, and also to the span of the laminate. In order to pursue the so-called effect, some consumers require the designer to make some cabinet laminates to be particularly large, regardless of whether What board, most of the time is going to bend.
The bookcase span of this effect map will definitely be bent in actual use, the image source network, and the deletion.
Water swelling rate
I believe that everyone can also know from the literal meaning, this attribute is to represent your cabinet "proof against the tide."
But here we must correct a point of view, no matter what type of plate, which brand, what kind of craft is afraid of water! ! !
If you want to be afraid of blisters, there are two kinds of cabinets, one is brick/cement and the other is stainless steel cabinet!
Therefore, for the board, the moisture-proof is only to ensure that the relatively large air moisture content in the kitchen (there may be a small amount of water in the sink cabinet) will not swell and deform, affecting the balance of the force on the table and the nail holding force of the hinge. This removal is related to the water swell expansion rate of the sheet, and is also related to the edge sealing process after the sheet is cut.
It is recommended that you pay attention to two points when buying cabinets:
Whether the board used in the cabinet meets the national standard for water absorption expansion (less than 8%); roughly look at the edge-sealing process of the sample cabinet of the purchased cabinet: observe whether the edge is flat, whether there is overflow, whether it is falling off, etc.
Formaldehyde emission
All countries in the world have strict regulations on the amount of formaldehyde released from wood-based panels. "E0" is a more stringent grade mark for the release of formaldehyde from wood-based panels and their products. It is not a complete foreign product, but has distinctive Chinese characteristics.
At present, the so-called "E0 grade" national standard is found in the "impregnated paper laminated wood floor" GB/T 18102-2007, the standard is formaldehyde content ≤ 0.5mg / l, equivalent to the Japanese JAS star standard F ★ ★ ★ (≤ 0.5mg/L).
Regarding the environmental protection issues of various wood-based panels, there is nothing wrong with appointing well-known brands. Some environmentally-friendly brand plates may even exceed the so-called E0. To do things with these plates, there is no need to worry about environmental protection. If some brands use unknown plates, and even the sales staff is vague and unclear about the origin of the plates, please be careful to buy them. Some of the news about formaldehyde poisoning that you have seen is generally derived from this brand without brand. Small workshop plates.
Grip force
The screw force is the screw that is not easy to loosen, fall off, or blast after the screw is placed inside the plate.
For the cabinets we installed in our homes, the strength of the gripping force means that during the next at least one or twenty years of use, the hinge will not loosen or even fall, the drawer screws will loose, and the noise will be abnormal. Will the body structure be deformed?
When everyone buys custom furniture, how do you judge the strength of the nail holding?
The quality inspection report is certainly one of the important ways, but the most intuitive way is very simple, just ask the brand's sales, they can not sit up after their cabinet door is open. Of course, don't go up yourself! Although this method is not rigorous, the weight of the door drawer and the quality of the hinged drawer track also have a great relationship, but this is indeed the most straightforward way.
Jianjun Wood has been engaged in the sales of sheet metal for more than 20 years. As a professional supplier of early production and sales of ecological board, its sales of well-known brands such as Penghong, Meilunbao and Kumquat Tree have far higher quality requirements than ordinary plates. Products, is the best choice for your decoration, call 400---1166---921 for details, click to enter the mall, learn more!

Sauce Dispenser

Sauce Pump,Condiment Pump,Server Sauce Pump,Industrial Sauce Pump

Jiangmen Junerte Stainless Steel Kitchenware Co.,Ltd , https://www.junertejm.com